Thermal Properties Metric English Comments
CTE, linear 58.0 µm/m-°C

@Temperature -55.0 - 288 °C
32.2 µin/in-°F

@Temperature -67.0 - 550 °F
Z-Direction; ASTM D3386-94
Rogers Corporation RO3203 Woven-Glass Reinforced PTFE Laminate
Features and Benefits:Woven glass reinforcement - Improves rigidity for easier handlingUniform electrical and mechanical performance - ideal for complex multi-layer high frequency structuresLow diel..
CTE, linear 58.0 µm/m-°C

@Temperature <=100 °C
32.2 µin/in-°F

@Temperature <=212 °F
ISO E 830
Wolf Kunststoff ZEDEX® ZX-324V11T A3L PEEK Polymer, Reinforced
Main Charactistics: Stress resistant; High impact strength at 196 ° C Applications: Shipbuilding; Chemical Engineering; Automitve Technology; Machine ToolsInformation provided by Zedex
CTE, linear 58.0 µm/m-°C

@Temperature <=150 °C
32.2 µin/in-°F

@Temperature <=302 °F
ISO E 831
Wolf Kunststoff ZEDEX® ZX-324V11T A3L PEEK Polymer, Reinforced
Main Charactistics: Stress resistant; High impact strength at 196 ° C Applications: Shipbuilding; Chemical Engineering; Automitve Technology; Machine ToolsInformation provided by Zedex
CTE, linear 58.0 µm/m-°C

@Temperature <=150 °C
32.2 µin/in-°F

@Temperature <=302 °F
ISO E 831
Wolf Kunststoff ZEDEX® ZX-410 A4A Polymer Alloy
ZX-410 is a bearing material with excellent properties and a very affordable price.Main Characteristics: Hard, Stiff, Tough; High dimensional stability; High chemical resistance; High water resistan..
CTE, linear 58.0 µm/m-°C

@Temperature -118 - -54.0 °C
32.2 µin/in-°F

@Temperature -180 - -65.2 °F
Tra-Con Tra-Bond 832-5 Flexible Epoxy
TRA-BOND 832-5 is a flexible two component epoxy which is intended for bonding materials with mis-matched coefficients of expansion. It exhibits flexibility associated with polyurethanes but does no..
CTE, linear 58.0 µm/m-°C

@Temperature -40.0 - 0.000 °C
32.2 µin/in-°F

@Temperature -40.0 - 32.0 °F
ASTM E831-00
DSM Somos® ProtoTherm™ 12110 Water-resistant resin for stereolithography, UV Postcure
DescriptionDSM Somos® 12110 is a liquid photopolymer that produces strong, high temperature tolerant, water-resistant parts. Parts created with Somos® 12110 have a cherry-red appearance which tur..
CTE, linear 58.0 µm/m-°C

@Temperature <=40.0 °C
32.2 µin/in-°F

@Temperature <=104 °F
below Tg
Resinlab® SEC1233 Silver Filled Epoxy Adhesive
Resinlab™ SEC1233 is a silver filled, two component, room temperature curing epoxy adhesive. It is designed to cure completely at room temperature. SEC1233 provides excellent electrical conductivit..