Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear = 59.4 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 107 µm/m-°C

@Temperature 0.000 - 20.0 °C
59.4 µin/in-°F

@Temperature 32.0 - 68.0 °F
T<Tg; ASTM E831-93
Proto3000 Accura® 25 Plastic Stereolithography (SLA) Prototyping Polymer
Description: A high stiffness engineered nanocomposite that opens new applications for stereolithography users. Features: Look and feel of molded polypropyleneOutstanding feature resolution and accu..
CTE, linear 107 µm/m-°C

@Temperature <=150 °C
59.4 µin/in-°F

@Temperature <=302 °F
ISO E 831
Wolf Kunststoff ZEDEX® ZX-100MT A1T Polymer Alloy, Mineral Reinforced
Stiff; Hard; Very high strength; No fiber reinforcementApplications: Handling, Vessel and Pump, Steel and Water, Chemical Engineering, Automotive Technology, Machine ToolsInformation provided by Zed..
CTE, linear 107 µm/m-°C

@Temperature 0.000 - 20.0 °C
59.4 µin/in-°F

@Temperature 32.0 - 68.0 °F
T<Tg; ASTM E831-93
3D Systems Accura® 25 Plastic for SLA® Systems
For use with solid-state stereolithography (SLA®) systems.ApplicationsFunctional components for assemblies and mock-ups for:Automotive styling parts — trim, fascia, and other componentsConsumer el..