Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 11.5 µm/m-°C @Temperature 20.0 - 300 °C |
6.39 µin/in-°F @Temperature 68.0 - 572 °F |
|
Kennametal Stellite Stellite® 98M2 cast Adhesive wear test data P/M 0.58 Typical applications include vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, saw.. |
|||
CTE, linear | 11.5 µm/m-°C @Temperature 25.0 - 100 °C |
6.39 µin/in-°F @Temperature 77.0 - 212 °F |
|
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Bar, Hot Rolled and Solution Annealed HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
CTE, linear | 11.5 µm/m-°C @Temperature 25.0 - 100 °C |
6.39 µin/in-°F @Temperature 77.0 - 212 °F |
|
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Shielded Metal Arc Welded (SMAW) Plate HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
CTE, linear | 11.5 µm/m-°C @Temperature 20.0 - 93.0 °C |
6.39 µin/in-°F @Temperature 68.0 - 199 °F |
|
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 649°C (1200°F), aged 8000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
CTE, linear | 11.5 µm/m-°C @Temperature 20.0 - 93.0 °C |
6.39 µin/in-°F @Temperature 68.0 - 199 °F |
|
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 760°C (1400°F), aged 8000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
CTE, linear | 11.5 µm/m-°C @Temperature 20.0 - 93.0 °C |
6.39 µin/in-°F @Temperature 68.0 - 199 °F |
|
Haynes Hastelloy® S alloy, gas tungsten arc welded Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
CTE, linear | 11.5 µm/m-°C @Temperature 20.0 - 93.0 °C |
6.39 µin/in-°F @Temperature 68.0 - 199 °F |
|
Haynes Hastelloy® S alloy, plate 12.7 mm (1/2 in.) thick, solution heat-treated at 427°C (800°F), aged 1000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
CTE, linear | 11.5 µm/m-°C @Temperature 20.0 - 93.0 °C |
6.39 µin/in-°F @Temperature 68.0 - 199 °F |
|
Haynes Hastelloy® S alloy, weld metal, aged 1000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
CTE, linear | 11.5 µm/m-°C @Temperature 20.0 - 93.0 °C |
6.39 µin/in-°F @Temperature 68.0 - 199 °F |
|
Haynes Hastelloy® S alloy, weld metal, aged 16000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
CTE, linear | 11.5 µm/m-°C @Temperature 20.0 - 93.0 °C |
6.39 µin/in-°F @Temperature 68.0 - 199 °F |
|
Haynes Hastelloy® S alloy, weld metal, aged at 649°C (1200°F) for 1000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
CTE, linear | 11.5 µm/m-°C @Temperature 20.0 - 427 °C |
6.39 µin/in-°F @Temperature 68.0 - 801 °F |
|
HP Alloys Alloy B-2, Solution Treated, 10% Cold Worked Solution Treated, 10% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International. |
|||
CTE, linear | 11.5 µm/m-°C @Temperature 20.0 - 427 °C |
6.39 µin/in-°F @Temperature 68.0 - 801 °F |
|
HP Alloys Alloy B-2, Solution Treated, 30% Cold Worked Solution Treated, 30% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International. |
|||
CTE, linear | 11.5 µm/m-°C @Temperature 20.0 - 260 °C |
6.39 µin/in-°F @Temperature 68.0 - 500 °F |
|
Crucible Steel CPM® Rex® 54® (HS) High Speed Steel CPM Rex 54 is a cobalt-bearing high speed steel designed to offer an improvement in the red hardness of the popular M4 grade, while maintaining wear properties equivalent to M4. CPM Rex 54 has a che.. |
|||
CTE, linear | 11.5 µm/m-°C @Temperature 20.0 - 260 °C |
6.39 µin/in-°F @Temperature 68.0 - 500 °F |
|
Crucible Steel PM M2 Tool Steel PM M2 is an improved quality tool steel compared to conventionally produced material. The powder metallurgy process results in a homogeneous microstructure exhibiting a uniform distribution of fine .. |
|||
CTE, linear | 11.5 µm/m-°C @Temperature 200 °C |
6.39 µin/in-°F @Temperature 392 °F |
|
Bohler-Uddeholm BÖHLER S401(M1) High Speed Steel Description: Molybdenum high speed steel with high toughness and good cutting ability. Applications: Taps, twist drills, reamers, milling tools, broaches toolsStandards: DIN/EN 1.3346 HS2-91, AISI M.. |
|||
CTE, linear | 11.5 µm/m-°C @Temperature 20.0 - 100 °C |
6.39 µin/in-°F @Temperature 68.0 - 212 °F |
|
Bohler-Uddeholm BÖHLER W302 SUPERIOR® Premium H13 Tool Steel A premium grade H13 hot work tool steel featuring:Very good toughness properties meeting the requirements of NADCA 207-97, and the superior quality levels of NADCA 207-2003Very good heat checking re.. |
|||
CTE, linear | 11.5 µm/m-°C @Temperature 100 °C |
6.39 µin/in-°F @Temperature 212 °F |
|
Bohler-Uddeholm BÖHLER W303 ISODISC® Hot Work Tool Steel Description: Hot work tool steel featuring excellent hot tensile properties, high retention of hardness, good toughness and resistance to heat checking, admits water cooling. BOHLER W303 is also ava.. |
|||
CTE, linear | 11.5 µm/m-°C @Temperature 20.0 - 100 °C |
6.39 µin/in-°F @Temperature 68.0 - 212 °F |
|
Bohler-Uddeholm BÖHLER W403 VMR® Hot Work Tool Steel W403 VMR is a modified hot work alloy with an excellent combination of hot tensile properties and toughness. The balanced properties of this grade are not only due to chemistry modification, but to .. |
|||
CTE, linear | 11.5 µm/m-°C @Temperature 23.0 - 427 °C |
6.39 µin/in-°F @Temperature 73.4 - 801 °F |
|
Carpenter Chrome Core® 18-FM Solenoid Quality Stainless Steel, Stress Relieved Data provided by Carpenter Technology Corporation.This is a soft ferritic material designed for operation in more corrosive environments than tolerated by 18% Cr-Fe Type 430 stainless. This new mat.. |
|||
CTE, linear | 11.5 µm/m-°C @Temperature 20.0 - 500 °C |
6.39 µin/in-°F @Temperature 68.0 - 932 °F |
|
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 416, Tempered at 482°C (UNS S41600) Allegheny Ludlum's 416 is a free-machining stainless steel specifically designed to exhibit improved machinability. These modifications retain, in so far as possible, the good mechanical properties.. |
|||
CTE, linear | 11.5 µm/m-°C @Temperature 20.0 - 500 °C |
6.39 µin/in-°F @Temperature 68.0 - 932 °F |
|
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 416, Tempered at 593°C (UNS S41600) Allegheny Ludlum's 416 is a free-machining stainless steel specifically designed to exhibit improved machinability. These modifications retain, in so far as possible, the good mechanical properties.. |
|||
CTE, linear | 11.5 µm/m-°C @Temperature 20.0 - 200 °C |
6.39 µin/in-°F @Temperature 68.0 - 392 °F |
|
Bohler-Uddeholm BÖHLER W360 ISOBLOC® Hot Work Tool Steel BÖHLER W360 ISOBLOC was developed as a tool steel for dies and punches in warm and hot forging. The steel can be used for a variety of applications where hardness and toughness are required. Prope.. |
|||
CTE, linear | 11.5 µm/m-°C @Temperature 20.0 - 500 °C |
6.39 µin/in-°F @Temperature 68.0 - 932 °F |
|
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 416, Tempered at 704°C (UNS S41600) Allegheny Ludlum's 416 is a free-machining stainless steel specifically designed to exhibit improved machinability. These modifications retain, in so far as possible, the good mechanical properties.. |
|||
CTE, linear | 11.5 µm/m-°C @Temperature 20.0 - 93.0 °C |
6.39 µin/in-°F @Temperature 68.0 - 199 °F |
|
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 649°C (1200°F), aged 1000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Applications .. |
|||
CTE, linear | 11.5 µm/m-°C @Temperature 21.0 - 316 °C |
6.39 µin/in-°F @Temperature 69.8 - 601 °F |
|
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 1025 (Heated 552°C) Data provided by Carpenter Technology Corporation.Custom 630 (17Cr-4Ni) is a martensitic precipitation/age-hardening stainless steel offering high strength and hardness along with excellent corrosio.. |