Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 11.5 µm/m-°C @Temperature 20.0 - 299 °C |
6.40 µin/in-°F @Temperature 68.0 - 570 °F |
|
Schmolz + Bickenbach UgiPermâ„¢ 12FM Stainless Steel Bar Description: UgiPermâ„¢ 12FM is a 12% chrome ferritic stainless with improved magnetic properties designed for use in electro-injectors, valves and many other applications. The grade was develope.. |
|||
CTE, linear | 11.5 µm/m-°C @Temperature 20.0 - 399 °C |
6.40 µin/in-°F @Temperature 68.0 - 750 °F |
|
EDRO #8 Premium 420 Stainless Mold Steel EDRO #8™ is a chromium-alloyed stainless tool steel with the following properties: excellent corrosion resistance, superior polishability, good wear resistance, good machinability, and stability in.. |
|||
CTE, linear | 11.5 µm/m-°C @Temperature 21.1 - 204 °C |
6.40 µin/in-°F @Temperature 70.0 - 400 °F |
|
Crucible Steel 161 Tool Steel, High Carbon H13 Crucible 161 is a high carbon modification of H13, intended for applications requiring higher hardness, compressive strength, wear resistance, or tempering resistance (hot hardness), at slightly low.. |
|||
CTE, linear | 11.5 µm/m-°C @Temperature 21.1 - 204 °C |
6.40 µin/in-°F @Temperature 70.0 - 400 °F |
|
Crucible Steel CPM® Nu-Die® EZ Tool Steel CRUCIBLE CPM Nu-Die EZ is a new, patented die and mold steel designed for service as die casting dies and plastic injection molds. It is supplied in the prehardened condition, and is easily machined.. |
|||
CTE, linear | 11.5 µm/m-°C @Temperature 21.1 - 593 °C |
6.40 µin/in-°F @Temperature 70.0 - 1100 °F |
|
Crucible Steel CPM® REX® M35HCHS High Speed Steel, AISI M35 CPM REX M35HCHS is a 5% cobalt modification of M2 high speed steel used almost exclusively for hobs and other gear cutting tools where higher red hardness is required. Made by the Crucible Particle .. |
|||
CTE, linear | 11.5 µm/m-°C @Temperature 21.1 - 260 °C |
6.40 µin/in-°F @Temperature 70.0 - 500 °F |
|
Crucible Steel REX® M2 S 1.0C High Speed Steel, AISI M2 REX M2S (1.0C) is a sulfur-bearing high carbon version of the regular CRUCIBLE REX M2 high speed steel. The sulfur addition provides good grindability and an improvement in machinability of 25 to 35.. |
|||
CTE, linear | 11.5 µm/m-°C @Temperature 21.1 - 260 °C |
6.40 µin/in-°F @Temperature 70.0 - 500 °F |
|
Crucible Steel REX® M2 S High Speed Steel REX M2 is a tungsten-molybdenum high speed steel which gives outstanding performance in all operations where a general purpose high speed steel is required. REX M2 has a wide hardening range, excell.. |
|||
CTE, linear | 11.5 µm/m-°C @Temperature 21.1 - 260 °C |
6.40 µin/in-°F @Temperature 70.0 - 500 °F |
|
Crucible Steel REX® M3-1 High Speed Steel, AISI M3-1 REX M3-1 is a lower carbon, lower vanadium modification of M3-2 high speed steel. This lower alloy content results in better machining and grinding characteristics compared to M3-2, with a slight im.. |
|||
CTE, linear | 11.5 µm/m-°C @Temperature 399 °C |
6.40 µin/in-°F @Temperature 750 °F |
hardened to 52 HRC |
Bohler-Uddeholm POLMAX® 420 Modified - Stainless Mold Steel Polmax is an excellent choice for extreme surface finish requirements. This high performance grade achieves surface finishes that go well beyond conventional tool steels. Polmax is specifically eng.. |
|||
CTE, linear | 11.5 µm/m-°C @Temperature 93.3 - 204 °C |
6.40 µin/in-°F @Temperature 200 - 400 °F |
|
Crucible Steel PDCQ Premium Quality High Toughness H13 Steel Crucible PDCQ™ is a premium version of H13, manufactured to exceed die casting industry specifications. PDCQ has at least 10 ft. lbs room temperature transverse toughness. Its enhanced toughness pr.. |
|||
CTE, linear | 11.5 µm/m-°C @Temperature 21.1 - 204 °C |
6.40 µin/in-°F @Temperature 70.0 - 400 °F |
|
Schmolz + Bickenbach Formadur® 2083 Superclean Plastic Mold Steel Description: Formadur 2083 Superclean is an electro slag remelted (ESR) martensitic stainless steel developed for corrosion resistant applications and Supplied in the annealed conditionCharacteristi.. |
|||
CTE, linear | 11.5 µm/m-°C @Temperature 21.1 - 288 °C |
6.40 µin/in-°F @Temperature 70.0 - 550 °F |
|
Schmolz + Bickenbach Formadur® 2083 Superclean Plastic Mold Steel Description: Formadur 2083 Superclean is an electro slag remelted (ESR) martensitic stainless steel developed for corrosion resistant applications and Supplied in the annealed conditionCharacteristi.. |