Polymer Property : CTE, linear = 6.800 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 12.24 µm/m-°C

@Temperature 38.0 - 649 °C
6.800 µin/in-°F

@Temperature 100 - 1200 °F
Latrobe DuraTechâ„¢ M4 High Carbon Powder Metal High Speed Steel (ASTM M4)
DuraTech M4 high speed steel is an extremely versatile high speed steel which provides a unique combination of high wear resistance with high impact toughness and transverse bend strength. A large v..
CTE, linear 12.24 µm/m-°C

@Temperature 38.0 - 649 °C
6.800 µin/in-°F

@Temperature 100 - 1200 °F
Latrobe DuraTechâ„¢ M4 Powder Metal High Speed Steel (ASTM M4)
DuraTech M4 high speed steel is an extremely versatile high speed steel which provides a unique combination of high wear resistance with high impact toughness and transverse bend strength. A large v..
CTE, linear 12.24 µm/m-°C

@Temperature 20.0 - 540 °C
6.800 µin/in-°F

@Temperature 68.0 - 1000 °F
Crucible Steel CPM® Rex® 20® (HS) High Speed Steel
CPM Rex 20 is a cobalt-free super high speed steel made by the CPM (Crucible Particle Metallurgy) Process. It has heat treat response and red hardness comparable to that of M42 but offers better wea..