Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 12.54 µm/m-°C @Temperature 21.0 - 358 °C |
6.967 µin/in-°F @Temperature 69.8 - 676 °F |
|
Latrobe HS-29XLâ„¢ ASTM M2-HC High Speed Steel HS-29XL (M2-HC) is the M2 composition with the carbon content increased and with the addition of alloy sulfides. The higher carbon content provides higher hardness and
superior red hardness compared.. |
|||
CTE, linear | 12.54 µm/m-°C @Temperature 21.0 - 358 °C |
6.967 µin/in-°F @Temperature 69.8 - 676 °F |
|
Latrobe Double Six™ ASTM M2 High Speed Steel DOUBLE SIX (M2) is a tungsten-molybdenum high speed steel with a well balanced composition suitable for a wide variety of applications. World wide, the M2 type is by far
the most popular high speed .. |