Thermal Properties Metric English Comments
CTE, linear 12.59 µm/m-°C

@Temperature 25.0 - 200 °C
6.994 µin/in-°F

@Temperature 77.0 - 392 °F
Carpenter S7 Alloy Tool Steel (AISI S7)
Carpenter S7 is a general purpose air hardening tool steel having high impact and shock resistance. It has good resistance to softening at moderately high temperatures. This combination of propertie..