Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 115 µm/m-°C @Temperature >=143 °C |
63.9 µin/in-°F @Temperature >=289 °F |
Average above Tg; ISO 11359 |
Victrex® PEEK 450FC30 General Purpose Product Description: High performance thermoplastic material, 30% reinforced with carbon fibre / graphite / PTFE PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and ext.. |