Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 69.4 µm/m-°C @Temperature -40.0 - 0.000 °C |
38.6 µin/in-°F @Temperature -40.0 - 32.0 °F |
ASTM E831-05 |
DSM Somos® ProtoGen™ 18920 Liquid Photopolymer, UV Postcure Product DescriptionDSM Somos® ProtoGen 18920 is a liquid photopolymer that produces accurate, ABS-like parts ideal for general purpose applications. ProtoGen resins are the first SL resins to demo.. |