Polymer Property : CTE, linear = 7.322 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 13.18 µm/m-°C

@Temperature 649 °C
7.322 µin/in-°F

@Temperature 1200 °F
Special Metals INCOLOY® alloy 908
INCOLOY® alloy 908 (UNS N09908) is an age-hardenable nickel-iron alloy which exhibits a low coefficient of thermal expansion, high tensile strength, high fracture and impact toughness, fatigue cr..
CTE, linear 13.18 µm/m-°C

@Temperature 25.0 - 316 °C
7.322 µin/in-°F

@Temperature 77.0 - 601 °F
Mean
Special Metals INCONEL® MA758 Oxide-Dispersion-Strengthened Ni-Cr Superalloy
Data provided by the manufacturer, Special Metals.
CTE, linear 13.18 µm/m-°C

@Temperature 0.000 - 100 °C
7.322 µin/in-°F

@Temperature 32.0 - 212 °F
Carpenter BioDur™ CCM® Medical Implant Alloy, Annealed
Data provided by Carpenter Technology Corporation.Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting high strength, corrosion resistance, and wear resistance. BioDur Carpenter CCM alloy..
CTE, linear 13.18 µm/m-°C

@Temperature 0.000 - 100 °C
7.322 µin/in-°F

@Temperature 32.0 - 212 °F
Carpenter BioDur™ CCM® Medical Implant Alloy, Warm Worked
Data provided by Carpenter Technology Corporation.Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting high strength, corrosion resistance, and wear resistance. BioDur Carpenter CCM alloy..
CTE, linear 13.18 µm/m-°C

@Temperature 0.000 - 100 °C
7.322 µin/in-°F

@Temperature 32.0 - 212 °F
Carpenter BioDur™ CCM® Medical Implant Alloy, Hot Worked
Data provided by Carpenter Technology Corporation.Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting high strength, corrosion resistance, and wear resistance. BioDur Carpenter CCM alloy..