Thermal Properties Metric English Comments
CTE, linear 14.27 µm/m-°C

@Temperature 500 °C
7.928 µin/in-°F

@Temperature 932 °F
Special Metals INCONEL® alloy 740 Precipitation-Hardenable Ni-Cr-Co Superalloy
INCONEL® alloy 740 is a nickel-chromium-cobalt alloy developed by Special Metals Corporation. The alloy is age hardenable by the precipitation of a gamma prime second phase. Potential applicati..
CTE, linear 14.27 µm/m-°C

@Temperature 25.0 - 700 °C
7.928 µin/in-°F

@Temperature 77.0 - 1290 °F
Carpenter S7 Alloy Tool Steel (AISI S7)
Carpenter S7 is a general purpose air hardening tool steel having high impact and shock resistance. It has good resistance to softening at moderately high temperatures. This combination of propertie..