Thermal Properties Metric English Comments
CTE, linear 74.6 - 75.5 µm/m-°C

@Temperature -40.0 - 0.000 °C
41.4 - 41.9 µin/in-°F

@Temperature -40.0 - 32.0 °F
ASTM E831-00
DSM Somos® ProtoGen™ O-XT 18420 Epoxy Resin for Stereolithography, UV Postcure at HOC -2
DescriptionDSM Somos® ProtoGen O-XT 18420 is a liquid, ABS-like, photopolymer that produces accurate parts ideal for general purpose applications. ProtoGen resins are the first SL resins to demons..