Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 15.03 µm/m-°C @Temperature 1400 °C |
8.350 µin/in-°F @Temperature 2550 °F |
|
Special Metals INCONEL® alloy MA758 Ni-Cr Superalloy INCONEL® alloy MA 758 is an oxide-dispersion-strengthened (ODS) nickel-chromium superalloy, made by mechanical alloying. It is a development of the well-established aerospace superalloy, INCONEL.. |
|||
CTE, linear | 15.03 µm/m-°C @Temperature 25.0 - 760 °C |
8.350 µin/in-°F @Temperature 77.0 - 1400 °F |
Mean |
Special Metals INCONEL® MA758 Oxide-Dispersion-Strengthened Ni-Cr Superalloy Data provided by the manufacturer, Special Metals. |