CTE, linear 8.70 µm/m-°C

@Temperature 20.0 - 300 °C
4.83 µin/in-°F

@Temperature 68.0 - 572 °F
H.C. Starck WCu 80/20 Tungsten-Copper Composite Material
Description of Product: Tungsten-copper composite materials are produced by copper infiltration of porous sintered tungsten. They are available with different copper contents (10 - 30 %). A therm..
CTE, linear 8.70 µm/m-°C

@Temperature 20.0 - 300 °C
4.83 µin/in-°F

@Temperature 68.0 - 572 °F
Schott BG42 Band Pass Filter
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.
CTE, linear 8.70 µm/m-°C

@Temperature 20.0 - 300 °C
4.83 µin/in-°F

@Temperature 68.0 - 572 °F
Schott N-BASF64 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 8.70 µm/m-°C

@Temperature 20.0 - 1000 °C
4.83 µin/in-°F

@Temperature 68.0 - 1830 °F
DIN EN 821-1
CeramTec B 601 Alumina, 98.5%
Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at elevated temperatures.
CTE, linear 8.70 µm/m-°C

@Temperature 20.0 - 1000 °C
4.83 µin/in-°F

@Temperature 68.0 - 1830 °F
DIN EN 821-1
CeramTec B 40 Alumina, 99.1%
B 40 is the ideal sliding mate with the same properties as Rubalit® A 1896. It contains a larger share of Al2O3 for superior chemical stability.
CTE, linear 8.70 µm/m-°C

@Temperature -30.0 - 70.0 °C
4.83 µin/in-°F

@Temperature -22.0 - 158 °F
Schott BG28 Band Pass Filter
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.
CTE, linear 8.70 µm/m-°C

@Temperature -30.0 - 70.0 °C
4.83 µin/in-°F

@Temperature -22.0 - 158 °F
Schott BG25 Band Pass Filter
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.