Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 148 µm/m-°C @Temperature >=149 °C |
82.0 µin/in-°F @Temperature >=300 °F |
ASTM E228 |
Greene Tweed Arlon® 1330 PEEK Arlon® is a tough, high-temperature, semi-crystalline, thermoplastic presenting a unique combination of mechanical, thermal, chemical and electrical properties. Greene, Tweed uses several proprie.. |