CTE, linear 151 µm/m-°C

@Temperature 90.0 - 150 °C
83.9 µin/in-°F

@Temperature 194 - 302 °F
T>Tg; ASTM E831-93
Proto3000 Accura® 25 Plastic Stereolithography (SLA) Prototyping Polymer
Description: A high stiffness engineered nanocomposite that opens new applications for stereolithography users. Features: Look and feel of molded polypropyleneOutstanding feature resolution and accu..
CTE, linear 151 µm/m-°C

@Temperature 90.0 - 150 °C
83.9 µin/in-°F

@Temperature 194 - 302 °F
T>Tg; ASTM E831-93
3D Systems Accura® 25 Plastic for SLA® Systems
For use with solid-state stereolithography (SLA®) systems.ApplicationsFunctional components for assemblies and mock-ups for:Automotive styling parts — trim, fascia, and other componentsConsumer el..