CTE, linear 17.02 µm/m-°C

@Temperature 300 °C
9.456 µin/in-°F

@Temperature 572 °F
0.100-in Cold-Rolled Plate; ASTM E 228
Special Metals INCOLOY® alloy 832 Stainless Steel
INCOLOY® alloy 832 is a low cost stainless steel developed specifically for domestic and industrial sheathed heater applications. With specific chemistry additions to ensure satisfactory formula..