Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 9.60 µm/m-°C @Temperature 20.0 - 450 °C |
5.33 µin/in-°F @Temperature 68.0 - 842 °F |
|
H.C. Starck MoCu 65/35 Molybdenum-Copper Composite Material Description of Product: Molybdenum-copper composite materials are produced by copper infiltration of porous sintered molybdenum. They are available with different copper contents (15 - 35 %). A t.. |
|||
CTE, linear | 9.60 µm/m-°C @Temperature -30.0 - 70.0 °C |
5.33 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott FG13 Conversion Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz..Similar glasses include BG34, FG3 |
|||
CTE, linear | 9.60 µm/m-°C @Temperature 20.0 - 300 °C |
5.33 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott GG385 Long Pass Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG630.. |
|||
CTE, linear | 9.60 µm/m-°C @Temperature -30.0 - 70.0 °C |
5.33 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott OG590 Long Pass Filter Colloidally colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, GG385, RG610, RG6.. |
|||
CTE, linear | 9.60 µm/m-°C @Temperature -30.0 - 70.0 °C |
5.33 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott N-KF9 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 9.60 µm/m-°C @Temperature -30.0 - 70.0 °C |
5.33 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott N-PSK53A Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 9.60 µm/m-°C @Temperature -30.0 - 70.0 °C |
5.33 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott GG435 Long Pass Filter Colloidally colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG385, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG6.. |
|||
CTE, linear | 9.60 µm/m-°C @Temperature -30.0 - 70.0 °C |
5.33 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott GG455 Long Pass Filter Colloidally colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG385, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG6.. |
|||
CTE, linear | 9.60 µm/m-°C @Temperature -30.0 - 70.0 °C |
5.33 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott OG530 Long Pass Filter Colloidally colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG455, GG475, GG495, OG515, GG385, OG550, OG570, OG590, RG610, RG6.. |
|||
CTE, linear | 9.60 µm/m-°C @Temperature -30.0 - 70.0 °C |
5.33 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott RG665 Long Pass Filter Colloidally colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG6.. |
|||
CTE, linear | 9.60 µm/m-°C @Temperature -30.0 - 70.0 °C |
5.33 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott RG695 Long Pass Filter Colloidally colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG6.. |
|||
CTE, linear | 9.60 µm/m-°C @Temperature 100 °C |
5.33 µin/in-°F @Temperature 212 °F |
|
Bohler-Uddeholm BÖHLER S290 MICROCLEAN® High Speed Steel Description: High speed steel produced by powder-metallurgy methods with highest red hardness, compressive strength and wear resistance. The PM technology imparts to the material also excellent toug.. |
|||
CTE, linear | 9.60 µm/m-°C @Temperature -30.0 - 70.0 °C |
5.33 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott RG780 Long Pass Filter Colloidally colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG6.. |