Thermal Properties Metric English Comments
CTE, linear 16.3 - 17.3 µm/m-°C

@Temperature 20.0 - 300 °C
9.06 - 9.61 µin/in-°F

@Temperature 68.0 - 572 °F
PEAK Werkstoff DISPAL S220 Aluminum Alloy, AlSi35, Condition F
Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational..
CTE, linear 16.3 - 17.3 µm/m-°C

@Temperature 20.0 - 300 °C
9.06 - 9.61 µin/in-°F

@Temperature 68.0 - 572 °F
PEAK Werkstoff DISPAL S220 Aluminum Alloy, AlSi35, Condition O
Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational..
CTE, linear 16.3 - 17.3 µm/m-°C

@Temperature 20.0 - 300 °C
9.06 - 9.61 µin/in-°F

@Temperature 68.0 - 572 °F
PEAK Werkstoff DISPAL S226 Aluminum Alloy, AlSi30CuMg, Condition T6
Heat Treatment Condition T6 (Quench in water at RT)abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of p..
CTE, linear 16.3 - 17.3 µm/m-°C

@Temperature 20.0 - 300 °C
9.06 - 9.61 µin/in-°F

@Temperature 68.0 - 572 °F
PEAK Werkstoff DISPAL S270 Aluminum Alloy, AlSi25Fe4Ni3CuMgMnCrTi, Condition F
Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational..
CTE, linear 16.3 - 17.3 µm/m-°C

@Temperature 20.0 - 300 °C
9.06 - 9.61 µin/in-°F

@Temperature 68.0 - 572 °F
PEAK Werkstoff DISPAL S270 Aluminum Alloy, AlSi25Fe4Ni3CuMgMnCrTi, Condition T6
Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational..
CTE, linear 16.3 - 17.3 µm/m-°C

@Temperature 20.0 - 300 °C
9.06 - 9.61 µin/in-°F

@Temperature 68.0 - 572 °F
PEAK Werkstoff DISPAL S270 Aluminum Alloy, AlSi25Fe4Ni3CuMgMnCrTi, Condition T4
Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational..