Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 16.7 - 17.7 µm/m-°C @Temperature 20.0 - 100 °C |
9.28 - 9.83 µin/in-°F @Temperature 68.0 - 212 °F |
|
PEAK Werkstoff DISPAL S260 Aluminum Alloy, AlSi25Cu4Mg, Condition F Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |
|||
CTE, linear | 16.7 - 17.7 µm/m-°C @Temperature 20.0 - 100 °C |
9.28 - 9.83 µin/in-°F @Temperature 68.0 - 212 °F |
|
PEAK Werkstoff DISPAL S260 Aluminum Alloy, AlSi25Cu4Mg, Condition T7 Heat Treatment Condition T7 (Quenching in water at RT)Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allo.. |
|||
CTE, linear | 16.7 - 17.7 µm/m-°C @Temperature 20.0 - 100 °C |
9.28 - 9.83 µin/in-°F @Temperature 68.0 - 212 °F |
|
PEAK Werkstoff DISPAL S260 Aluminum Alloy, AlSi25Cu4Mg, Condition T6 Heat Treatment Condition T6 (Quenching in water at RT)Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allo.. |