Polymer Property : CTE, linear = 91.8 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 91.8 µm/m-°C

@Temperature 100 - 200 °C
51.0 µin/in-°F

@Temperature 212 - 392 °F
ASTM E831
3M Dyneon™ CCM605 PTFE, 25% Glass Filled  (discontinued **)
Type II, free flowing.Typical Applications: Finished or semi-finished parts: sheets, rods, tubes, billets for skiving of films or machining into complex shapes.Information provided by the Dyneon div..