Thermal Properties Metric English Comments
CTE, linear 149.9 - 167.1 µm/m-°C

@Temperature 100 - 150 °C
83.28 - 92.83 µin/in-°F

@Temperature 212 - 302 °F
ASTM E831-00
DSM Somos® WaterClear® Ultra 10122 Optically Clear, Colorless, Rigid, Stereolithography Resin
DescriptionDSM Somos® WaterClear Ultra 10122 is a next generation optically clear resin with ABS like properties and good temperature resistance. It produces colorless, functional, accurate parts ..