Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear = 93.3 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 168 µm/m-°C

@Temperature <=100 °C
93.3 µin/in-°F

@Temperature <=212 °F
ISO E 830
Wolf Kunststoff ZEDEX® ZX-100EL55 A1F Polymer Alloy, Elastomer Modified
Main Characteristics: Rubbery; Soft; High shock absorption; High impact resistance; Elongation > 300%Applications: Handling, Vessel and Pump, Steel and Water, Chemical Engineering, Automitve Technol..