Polymer Property : CTE, linear = 93.67 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 168.6 - 175.4 µm/m-°C

@Temperature 50.0 - 100 °C
93.67 - 97.44 µin/in-°F

@Temperature 122 - 212 °F
ASTM E831-05
DSM Somos® NeXT Stereolithography (SLA) Prototyping Polymer
Somos® NeXT combines stiffness and impact resistance which brings it close the performance of injection molded thermoplastics. It produces finished parts with tight tolerances and detailed features..