Thermal Properties Metric English Comments
CTE, linear 93.8 - 116.9 µm/m-°C

@Temperature 50.0 - 100 °C
52.1 - 64.94 µin/in-°F

@Temperature 122 - 212 °F
ASTM E831-00
DSM Somos® ProtoGen™ O-XT 18120 Epoxy Resin for Stereolithography, UV Postcure at HOC -2
DescriptionDSM Somos® ProtoGen O-XT 18120 is a liquid photopolymer that produces accurate parts ideal for general purpose applications. ProtoGen resins are the first SL resins to demonstrate diffe..