Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 84.7 - 95.3 µm/m-°C @Temperature 0.000 - 50.0 °C |
47.1 - 52.9 µin/in-°F @Temperature 32.0 - 122 °F |
ASTM E831-00 |
DSM Somos® ProtoGen™ O-XT 18120 Epoxy Resin for Stereolithography, UV Postcure at HOC -2 DescriptionDSM Somos® ProtoGen O-XT 18120 is a liquid photopolymer that produces accurate parts ideal for general purpose applications. ProtoGen resins are the first SL resins to demonstrate diffe.. |