Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 950 °C @Time 3600 sec |
1740 °F @Time 1.00 hour |
Homogeneous Heating |
Schott Nextrema® 712-6 Glass Ceramic The NEXTREMA® family of glass-ceramics combines the glossy appearance of glass with exceptional thermal, chemical, optical and mechanical properties such as:Very low coefficient of linear thermal.. |
|||
Maximum Service Temperature, Air | 950 °C @Time 3600 sec |
1740 °F @Time 1.00 hour |
Homogeneous Heating |
Schott Nextrema® 712-8 Glass Ceramic The NEXTREMA® family of glass-ceramics combines the glossy appearance of glass with exceptional thermal, chemical, optical and mechanical properties such as:Very low coefficient of linear thermal.. |
|||
Maximum Service Temperature, Air | 950 °C @Time 3600 sec |
1740 °F @Time 1.00 hour |
Homogeneous Heating |
Schott Nextrema® 724-8 Glass Ceramic The NEXTREMA® family of glass-ceramics combines the glossy appearance of glass with exceptional thermal, chemical, optical and mechanical properties such as:Very low coefficient of linear thermal.. |