Polymer Property : Maximum Service Temperature, Air = 750 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 750 °C

@Time 3600 sec
1380 °F

@Time 1.00 hour
Inhomogeneous Heating
Schott Nextrema® 712-3 Glass Ceramic
The NEXTREMA® family of glass-ceramics combines the glossy appearance of glass with exceptional thermal, chemical, optical and mechanical properties such as:Very low coefficient of linear thermal..
Maximum Service Temperature, Air 750 °C

@Time 3600 sec
1380 °F

@Time 1.00 hour
Inhomogeneous Heating
Schott Nextrema® 724-3 Glass Ceramic
The NEXTREMA® family of glass-ceramics combines the glossy appearance of glass with exceptional thermal, chemical, optical and mechanical properties such as:Very low coefficient of linear thermal..