Polymer Property : Maximum Service Temperature, Air = 752 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 400 °C

@Time 1.80e+7 sec
752 °F

@Time 5000 hour
Inhomogeneous Heating
Schott Nextrema® 712-6 Glass Ceramic
The NEXTREMA® family of glass-ceramics combines the glossy appearance of glass with exceptional thermal, chemical, optical and mechanical properties such as:Very low coefficient of linear thermal..