Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Maximum Service Temperature, Air = 90.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 90.0 °C

@Time 7.20e+7 sec
194 °F

@Time 20000 hour
Murtfeldt Murlubric® [FS] Oil Modified Nylon 6
Murlubric® is a modified cast polyamide that mineral oil is integrated into during polymerization. As a result, the material has self lubricating properties and retains its excellent characteristi..
Maximum Service Temperature, Air 90.0 °C

@Time 7.20e+7 sec
194 °F

@Time 20000 hour
Murtfeldt Murlubric® Oil Modified Nylon 6
Murlubric® is a modified cast polyamide that mineral oil is integrated into during polymerization. As a result, the material has self lubricating properties and retains its excellent characteristi..
Maximum Service Temperature, Air 90.0 °C

@Time 7.20e+7 sec
194 °F

@Time 20000 hour
Murtfeldt Murylon® 6 Cast Nylon 6
Murylon® 6 CAST has extremely low levels of residual stress thanks to the casting procedure used to produce it. This material is therefore ideally suited to extensively processed components.Specia..
Maximum Service Temperature, Air 90.0 °C

@Time 1.80e+7 sec
194 °F

@Time 5000 hour
Murtfeldt Murytal® C Blue [FS] Acetal Copolymer
Thanks to their extremely low absorption of moisture, Murytal® materials are ideally suited for use as electronic isolation components. A fine crystalline structure and high yield strength mean th..
Maximum Service Temperature, Air 90.0 °C

@Time 7.20e+7 sec
194 °F

@Time 20000 hour
Murtfeldt Murytal® ESD Acetal Copolymer, Conductive
Additives make this material conductive. The mechanical properties of the material are retained almost in their entirety. Special Properties:• High rigidity• Excellent ability to regain its form•..
Maximum Service Temperature, Air 90.0 °C

@Time 7.20e+7 sec
194 °F

@Time 20000 hour
Murtfeldt Murytal® H Acetal Homopolymer
In addition to the excellent properties of Murytal® C, Murytal® H is stronger and more rigid with a lower expansion coefficient.Special Properties:• High rigidity• Excellent ability to regain it..