Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 179 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 81.7 °C
179 °F
Unannealed (0.250 in); ASTM D648
Entec Hypel® PEHD.8/.962 HDPE  (discontinued **)
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente..
Deflection Temperature at 0.46 MPa (66 psi) 81.7 °C
179 °F
ASTM D648
CPC - Vycom VINTEC I® PVC Polyvinyl Chloride (PVC)
Vintec I is a normal impact, high corrosion resistant polyvinyl chloride (PVC) sheet. Because of its exceptional corrosion resistance, it is ideally suited for applications where maximum chemical re..
Deflection Temperature at 0.46 MPa (66 psi) 81.7 °C
179 °F
ASTM D648
CPC - Vycom VINTEC® II TYPE II PVC Polyvinyl Chloride (PVC)
Vintec II is a high impact, corrosion resistant polyvinyl chloride (PVC) sheet. Because of its excellent impact and ductility it is ideally suited for applications that require thermal forming or wh..
Deflection Temperature at 0.46 MPa (66 psi) 81.7 °C
179 °F
ASTM D648
ExxonMobil PP9122 Polypropylene Homopolymer
Product Description: A random copolymer resin designed for extrusion blow molding applications and thermoforming of medical and other specialty devices and packaging. It has excellent organoleptics..
Deflection Temperature at 0.46 MPa (66 psi) 81.7 °C
179 °F
Unannealed; ASTM D648
Entec Hypel® PEHD.7/.962 HDPE
Available in North America Features: Food Contact Acceptable and High DensityAgency Ratings: FDA 21 CFR 177.1520RoHS Compliant Form: Pellets Information provided by Entec
Deflection Temperature at 0.46 MPa (66 psi) 81.7 °C
179 °F
ASTM D648
CPC - Vycom Ultra White™ PVC Advanced, UV (Ultra Violet) resistant sheet
Ultra White is an advanced PVC formulation designed specifically for outdoor applications where resistance to ultraviolet (UV) degradation is critical. Tests show that Ultra White retards both surfa..