Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 213 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 210 - 213 °C
410 - 415 °F
Average value: 211 °C Grade Count:9
Overview of materials for Polyetherimide (PEI), 20% Glass Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 20% Glass Fiber". Specific grades with glass content between 15% and 24% are included. E..
Deflection Temperature at 0.46 MPa (66 psi) 210 - 213 °C
410 - 415 °F
Average value: 212 °C Grade Count:14
Overview of materials for Polyetherimide (PEI), 30% Glass Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 30% Glass Fiber". Specific grades with glass content between 25% and 34% are included. E..
Deflection Temperature at 0.46 MPa (66 psi) 210 - 213 °C
410 - 415 °F
Average value: 212 °C Grade Count:5
Overview of materials for Polyetherimide (PEI), Aramid Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, Aramid Fiber Filled". Each property range of values reported is minimum and maximum valu..