Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 265 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 130 - 265 °C
266 - 509 °F
Average value: 147 °C Grade Count:91
Overview of materials for Polycarbonate, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum a..
Deflection Temperature at 0.46 MPa (66 psi) 177 - 265 °C
350 - 509 °F
Average value: 250 °C Grade Count:90
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and ma..