Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 269 °C
516 °F
HDT B; Unannealed; ISO 75-2/B
Solvay Specialty Polymers Lavanta® 5115 WH224 Polyester, High Performance (HPP), 15% Glass Fiber
Lavanta® 5115 WH224 is a 15% glass fiber reinforced, high-performance polyester (HPP) injection molding grade developed specifically for HB LED packaging applications that utilize surface mount t..
Deflection Temperature at 0.46 MPa (66 psi) 269 °C
516 °F
ASTM D648
A. Schulman ComAlloy Voloy® 686 Nylon 6/6, Glass Fiber/Bead Reinforced, Nylon 6/6 Alloy, Flame Retardant, UL
Data provided by the manufacturer, ComAlloy International Company.45% Glass Fiber/Bead Reinforced. Halogen- and phosphorous-freeThe ComAlloy product line has been integrated into the A Schulman prod..