Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 210 - 304 °C
410 - 580 °F
Average value: 248 °C Grade Count:90
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum..