Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 326 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 326 °C

@Thickness 3.20 mm
619 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP THERMOCOMP LF002 PEEK
LNP* THERMOCOMP* LF002 is a compound based on Polyetheretherketone resin containing 10% Glass Fiber.