Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 171 - 179 °C
340 - 355 °F
Average value: 177 °C Grade Count:5
Overview of materials for Nylon 11 with 20% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are includ..