Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 438 °F
Polymer Property :
Deflection Temperature at 0.46 MPa (66 psi) =
438 °F
Product List
Thermal Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties
Metric
English
Comments
Deflection Temperature at 0.46 MPa (66 psi)
226
°C
438
°F
ASTM D648
Solvay Technyl® A218 Heat Stabilized Nylon 66
Information provided by Rhodia; Rhodia has been acquired by Solvay.