Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 545 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 250 - 285 °C
482 - 545 °F
Average value: 279 °C Grade Count:23
Overview of materials for Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled". Each property range of values reported is mini..