Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 595 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 313 °C
595 °F
Unannealed; ASTM D648
Solvay Specialty Polymers Amodel® A-4122 NL WH 905 Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-4122 NL resin is a 22% glass reinforced, high-reflectivity white grade of polyphthalamide (PPA), designed to provide high crystallinity when molded in water-cooled molds. This material exhi..
Deflection Temperature at 0.46 MPa (66 psi) 313 °C
595 °F
Unannealed; ASTM D648
Solvay Specialty Polymers Amodel® A-4122 NL WH 905 Polyphthalamide (PPA), 22% Glass Fiber
Amodel® A-4122 NL resin is a 22% glass reinforced, high-reflectivity white grade of polyphthalamide (PPA), designed to provide high crystallinity when molded in water-cooled molds. This material ..