Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 63.9 °C | 147 °F | Unannealed; ISO 75B-1, -2 |
LyondellBasell Hifaxâ„¢ ETA3081HS Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ ETA3081HS medium melt flow, 800 MPa flexural modulus, paintable thermoplastic elastomeric olefin (TEO) resin has balanced physical properties, moldability and paintability. .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 63.9 °C | 147 °F | Unannealed; ISO 75B-1, -2 |
LyondellBasell Hifaxâ„¢ RTA3263EUV/1 Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ RTA3263EUV/1 fractional melt flow, 1,700 MPa flexural modulus, UV-stabilized, mineral-filled, extrusion grade thermoplastic elastomeric olefin (TEO) resin has an excellent b.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 63.9 °C | 147 °F | ISO 75-2/B |
ExxonMobil HDPE HMA 018 High Density Polyethylene Resin Product Description: HMA 018 is an easy flow HDPE grade, characterized by high gloss and dimensional stability. Availability: Africa & Middle East, Asia Pacific and Europe Additive: Thermal Stabili.. |