Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 338 °C
640 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics LNP THERMOCOMP LC008E PEEK
LNP* THERMOCOMP* LC008E is a compound based on Polyetheretherketone resin containing 40% Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive.
Deflection Temperature at 0.46 MPa (66 psi) 338 °C

@Thickness 3.20 mm
640 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP THERMOCOMP LC008E PEEK
LNP* THERMOCOMP* LC008E is a compound based on Polyetheretherketone resin containing 40% Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive.
Deflection Temperature at 0.46 MPa (66 psi) 338 °C
640 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics LNP THERMOCOMP LC008E PEEK (Asia Pacific)
LNP* Thermocomp* LC008E is a compound based on Polyetheretherketone resin containing Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive.
Deflection Temperature at 0.46 MPa (66 psi) 338 °C

@Thickness 3.20 mm
640 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP THERMOCOMP LC008E PEEK (Asia Pacific)
LNP* Thermocomp* LC008E is a compound based on Polyetheretherketone resin containing Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive.