Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 89.4 °C | 193 °F | unannealed; injection molded; ASTM D648 |
Americas Styrenics STYRON™ A-TECH™ 1220 High-Impact Polystyrene Resin
(discontinued **) STYRON™ A-TECH™ 1220 advanced technology polystyrene resin is a high impact, high modulus resin for extrusion thermoforming applications. The improved durability of this resin allows potential do.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.4 °C | 193 °F | ASTM D648 |
A. Schulman POLYFLAM™ RABS 930-01 Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.4 °C | 193 °F | ASTM D648 |
A. Schulman POLYFLAM™ RABS 930-01 Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.4 °C | 193 °F | ASTM D648 |
A. Schulman POLYFLAM™ RABS 930-01 Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.4 °C | 193 °F | ASTM D648 |
A. Schulman POLYFLAM™ RABS 930-01 Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.4 °C | 193 °F | ASTM D648 |
A. Schulman POLYFLAM™ RABS 930-01 Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.4 °C | 193 °F | ASTM D648 |
A. Schulman POLYFLAM™ RABS 930-01 Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 89.4 °C | 193 °F | ASTM D648 |
Americas Styrenics EB6755 High Impact Polystyrene Product CharacteristicsGood Environmental Stress Crack Resistance (ESCR)Good practical toughnessDeep draw thermoforming capableGood low temperature impactFood Contact CompliantTypical ApplicationsPa.. |