Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 35.0 °C | 95.0 °F | ISO 75/Method Bf |
Premix Thermoplastics PRE-ELEC® CP 1316
(discontinued **) PRE-ELEC CP 1316 is a conductive thermoplastic compound based on a polyolefin copolymer. Conductivity is achieved by using special conductive carbon black. In addition to a very low electrical resis.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 35.0 °C | 95.0 °F | ISO 75 A |
Borealis Borsoft™ SF203CF Soft Polypropylene Copolymer for Extrusion Coating Borsoft SF203CF is a new statistic-heterophasic propylene-ethylene copolymer suitable for coating applications. Its polymer structure permits perfect adhesion to certain products. According to the.. |