Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 37.2 °C
99.0 °F
Molded and tested in accordance with ASTM D4976; ASTM D648
Dow 722 Linear Low Density Polyethylene (LDPE)
DOW Polyethylene 722 is a broad molecular weight distribution homopolymer designed to offer good impact strength and rack resistance, with excellent flexibility. Typical applications include caps/c..