Thermal Properties Metric English Comments
UL RTI, Electrical 65.6 - 220 °C
150 - 428 °F
Average value: 210 °C Grade Count:135
Overview of materials for Silicone Rubber
This property data is a summary of similar materials in the MatWeb database for the category "Silicone Rubber". Each property range of values reported is minimum and maximum values of appropriate Ma..
UL RTI, Electrical 65.6 °C
150 °F
File E54153
Arlon 25188T020 0.020" Uncured Silicone Rubber/Laminated ETFE Film
Design/Construction:Liner: 0.003" PTFE Coated FiberglassSide 1: Uncured Silicone RubberSubstrate: Laminated ETFE Film-treated for adhesionThis data represents typical values for the production ma..