Polymer Property : UL RTI, Mechanical with Impact = 70.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
UL RTI, Mechanical with Impact 70.0 °C
158 °F
UL 746B
SABIC Innovative Plastics Cycoloy® C2800 PC+ABS
Non-chlorinated and non-brominated flame retardant PC+ABS offering balanced flow and impact properties for various applications.
UL RTI, Mechanical with Impact 70.0 °C
158 °F
UL 746B
SABIC Innovative Plastics Cycoloy® C2800 PC+ABS (Asia Pacific)
Non-chlorinated and non-brominated flame retardant PC/ABS offering balanced flow and impact for various applications.
UL RTI, Mechanical with Impact 70.0 °C
158 °F
UL 746B
SABIC Innovative Plastics Cycoloy® C6600 PC+ABS
Nonbrominated, nonchlorinated FR PC+ABS with balanced flow, impact and hydrolytic stability for a wide variety of applications including business equipment, monitors, enclosures, among others.
UL RTI, Mechanical with Impact 70.0 °C
158 °F
UL 746B
SABIC Innovative Plastics Cycoloy® C6600 PC+ABS (Asia Pacific)
CYCOLOY C6600 is a FR PC+ABS of nonbrominated, nonchlorinated flame retardant systems with balanced flow, impact and hydrolytic stability for a wide variety of applications including business equipm..
UL RTI, Mechanical with Impact 70.0 °C
158 °F
UL 746B
SABIC Innovative Plastics Cycoloy® C6600 PC+ABS (Europe-Africa-Middle East)
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow for a wide variety of thin wall or large size applicat..
UL RTI, Mechanical with Impact 70.0 °C
158 °F
UL 746B
SABIC Innovative Plastics Cycoloy® C6850REC PC+ABS (Europe-Africa-Middle East)
PC+ABS Industrial quality. Flame retardant. Limited colors only (Black and Grey)This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
UL RTI, Mechanical with Impact 70.0 °C
158 °F
UL 746B
SABIC Innovative Plastics Cycoloy® CE3210 PC+ABS (Europe-Africa-Middle East)
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering high impact and excellent extrusion and thermoforming characteristics. Halogen free according ..
UL RTI, Mechanical with Impact 70.0 °C
158 °F
UL 746B
SABIC Innovative Plastics Cycoloy® CY5210 PC+ABS (Europe-Africa-Middle East)
CYCOLOY CY5210 is a flame retardant PC/ABS using non-chlorinated and non-brominated FR additives for injection moulding. CYCOLOY CY5210 has an improved hydrolytic stability with balanced flow and im..
UL RTI, Mechanical with Impact 70.0 °C
158 °F
UL 746B
LG Chemical AF312C ABS, Flame Retardant
Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical..
UL RTI, Mechanical with Impact 70.0 °C
158 °F
UL746-B
Shuman 791 Black and Custom Colors ABS-Flame Retardant
Long term thermal aging rated. Excellent flame retardancy, good impact strength, good chemical resistance, good wear and abrasion resistance.Data provided by the manufacturer.