Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical without Impact | 65.6 - 220 °C | 150 - 428 °F | Average value: 202 °C Grade Count:135 |
Overview of materials for Silicone Rubber This property data is a summary of similar materials in the MatWeb database for the category "Silicone Rubber". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
UL RTI, Mechanical without Impact | 65.6 °C | 150 °F | File E54153 |
Arlon 25188T020 0.020" Uncured Silicone Rubber/Laminated ETFE Film Design/Construction:Liner: 0.003" PTFE Coated FiberglassSide 1: Uncured Silicone RubberSubstrate: Laminated ETFE Film-treated for adhesionThis data represents typical values for the production ma.. |