Polymer Property : Pour Point = -14.8 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Pour Point -26.0 °C
-14.8 °F
Base Oil; ASTM D97
Nye Lubricants 113 (DMO) Delicate Machinery Oil
Information provided by Nye Lubricants.
Pour Point -26.0 °C
-14.8 °F
Base Oil; ASTM D97
Nye Lubricants UniFlor 8320 (UF) Synthetic Oil
Information provided by Nye Lubricants.
Pour Point -26.0 °C
-14.8 °F
Base Oil; ASTM D97
Nye Lubricants UniFlor 8322 (857A) (UF) Synthetic Oil
Information provided by Nye Lubricants.
Pour Point -26.0 °C
-14.8 °F
ASTM D97
ChevronTexaco ISO 680 Synthetic Wheel Motor Lubricant EP
FeaturesChevron Synthetic Wheel Motor Lubricants EP are superior quality industrial EP gear lubricants. Their advanced formulation provides superior load carrying and antiwear properties; protection..