Thermal Properties | Metric | English | Comments |
---|---|---|---|
Pour Point | <= -34.4 °C | <= -30.0 °F | D97 |
Paratherm Corporation Paratherm™ HR™ Heat Transfer Fluid Paratherm HR™ Heat Transfer Fluid is an alkylated-aromatic based heat transfer fluid formulated for closed loop liquid phase heating to 650°F in fired heaters and 675°F in waste heat recovery and.. |
|||
Pour Point | -34.4 °C | -30.0 °F | |
Lubriplate AC-0 Petroleum-Based Air Compressor Fluid Formulated to reduce carbon & varnish buildup. They contain fluid zinc to effectively fight friction & wear thus reducing heat & foaming. Available in six ISO grades.AC Series Air Compressor Oils ar.. |
|||
Pour Point | -34.4 °C | -30.0 °F | |
Lubriplate FMO 150 AW USP Mineral Oil-Based Food Machinery Grade Oil For use where a Class H-1 oil is required. Manufactured in nine ISO grades for a variety of applications. Anti-wear fortified. NOTE: FMO-350AW is also available in a red and orange color which helps.. |
|||
Pour Point | -34.4 °C | -30.0 °F | |
Lubriplate H0-0 Petroleum-Based Heavy-Duty Hydraulic Oil Formulated for superior performance, this series contains fluid zinc to effectively reduce ring & vane wear. Excellent anti-rust, anti-corrosion, anti-foam and anti-oxidation properties. High anilin.. |
|||
Pour Point | -34.4 °C | -30.0 °F | |
Lubriplate SPO-222 Petroleum-Based Gear, Bearing, & Recirculating Oil Petroleum-based oils specifically designed for industrial applications such as gear cases, bearings, chains, machine ways, and general oiling. These tacky lubricants will provide anti-wear lubricati.. |
|||
Pour Point | -34.4 °C | -30.0 °F | |
Lubriplate STO 4 Oil Food Machinery Oil Special, non-corrosive oil for lubricating stirrups on bottle filling machines. Class H-2.**Available in Bottles, Jugs, Pails, 1/4 Drums and DrumsH-1 Class Lubricants are manufactured with ingredien.. |
|||
Pour Point | -34.4 °C | -30.0 °F | |
Lubriplate NO.2 Petroleum-Based Machine Tool Oil Compounded to impart a unique load carrying film, exceptional lubricity, and anti-friction properties not found in conventional oils of the same viscosity. Machine Tool Oils are available in Bottles.. |
|||
Pour Point | -34.4 °C | -30.0 °F | |
ConocoPhillips SynXPA® 100 R&O Oil Description: Conoco SynXPA R&O Oil lubricates stationary and portable rotary compressors, as well as reciprocating compressors that operate in severe service. It is useful in single- and double-acti.. |
|||
Pour Point | -34.4 °C | -30.0 °F | |
ConocoPhillips SynXPA® 150 R&O Oil Description: Conoco SynXPA R&O Oil lubricates stationary and portable rotary compressors, as well as reciprocating compressors that operate in severe service. It is useful in single- and double-acti.. |
|||
Pour Point | -34.4 °C | -30.0 °F | |
ConocoPhillips 46 Super Hydraulic Oil Description: Conoco Super Hydraulic Oil is a high-quality antiwear hydraulic fluid formulated from premium Conoco hydrocracked base stocks to provide superior water separation, antiwear protection, .. |
|||
Pour Point | -34.4 °C | -30.0 °F | |
ConocoPhillips Hydroclear Diamond Class® 68 AW Turbine Oil Diamond Class AW Turbine Oil is a premium quality, rust and oxidation (R&O)-inhibited, antiwear turbine oil developed for use in geared and direct-drive gas turbines and steam turbines in severe ser.. |
|||
Pour Point | -34.4 °C | -30.0 °F | |
ConocoPhillips Hydroclear® 1 Ultra-clean multi-purpose R&O Oil, AGMA Lubricant No. 1 Description: Conoco Hydroclear Ultra-Clean Multipurpose R&O Oil is a rust- and oxidation-inhibited industrial oil with ashless wear protection formulated from premium Conoco hydrocracked base stocks.. |
|||
Pour Point | -34.4 °C | -30.0 °F | |
ConocoPhillips Hydroclear® 100 Gas Compressor Fluid Description: Conoco Hydroclear Gas Compressor Fluid is designed to lubricate rotary screw and reciprocating compressors in natural gas service. Conoco's high-quality hydrocracked base oil, combi.. |
|||
Pour Point | -34.4 °C | -30.0 °F | |
ConocoPhillips Hydroclear® 100 Multipurpose R&O Oil, AGMA Lubricant No. 3 Description: Conoco Hydroclear Multipurpose R&O Oil is a rust- and oxidationinhibited industrial oil with ashless wear protection formulated from premium Conoco hydrocracked base stocks. Hydroclear .. |
|||
Pour Point | -34.4 °C | -30.0 °F | |
ConocoPhillips Hydroclear® 2 Ultra-clean multi-purpose R&O Oil, AGMA Lubricant No. 2 Description: Conoco Hydroclear Ultra-Clean Multipurpose R&O Oil is a rust- and oxidation-inhibited industrial oil with ashless wear protection formulated from premium Conoco hydrocracked base stocks.. |
|||
Pour Point | -34.4 °C | -30.0 °F | |
ConocoPhillips Hydroclear® 46 Multipurpose R&O Oil, AGMA Lubricant No. 1 Description: Conoco Hydroclear Multipurpose R&O Oil is a rust- and oxidation inhibited industrial oil with ashless wear protection formulated from premium Conoco hydrocracked base stocks. Hydroclear.. |
|||
Pour Point | -34.4 °C | -30.0 °F | |
ConocoPhillips Hydroclear® 68 2 EP gear Oil Description: Conoco Hydroclear EP Gear Oil is a premium extreme-pressure industrial gear lubricant with superior deposit control. Hydroclear EP Gear Oil is specially formulated with proprietary addi.. |
|||
Pour Point | -34.4 °C | -30.0 °F | |
ConocoPhillips Hydroclear® 68 Multipurpose R&O Oil, AGMA Lubricant No. 2 Description: Conoco Hydroclear Multipurpose R&O Oil is a rust- and oxidationinhibited industrial oil with ashless wear protection formulated from premium Conoco hydrocracked base stocks. Hydroclear .. |
|||
Pour Point | -34.4 °C | -30.0 °F | |
ConocoPhillips Hydroclear® El Mar® 15W-40 Ashless Supreme Description: Conoco Hydroclear El Mar Ashless Supreme is a premium ashless natural gas engine oil formulated from exclusive Conoco hydrocracked base stock. Hydroclear El Mar Ashless Supreme is speci.. |
|||
Pour Point | -34.4 °C | -30.0 °F | |
ConocoPhillips Hydroclear® El Mar® 15W-40 Low Ash Heavy Duty Description: Conoco Hydroclear El Mar Low Ash Heavy Duty is a high-quality low ash natural gas engine oil formulated from exclusive Conoco hydrocracked base stock. Hydroclear El Mar Low Ash Heavy Du.. |
|||
Pour Point | -34.4 °C | -30.0 °F | |
ConocoPhillips Hydroclear® El Mar® 40 Ashless Supreme Description: Conoco Hydroclear El Mar Ashless Supreme is a premium ashless natural gas engine oil formulated from exclusive Conoco hydrocracked base stock. Hydroclear El Mar Ashless Supreme is speci.. |
|||
Pour Point | -34.4 °C | -30.0 °F | |
ConocoPhillips Hydroclear® El Mar® Low Ash Heavy Duty SAE 40 Description: Conoco Hydroclear El Mar Low Ash Heavy Duty is a high-quality low ash natural gas engine oil formulated from exclusive Conoco hydrocracked base stock. Hydroclear El Mar Low Ash Heavy Du.. |
|||
Pour Point | -34.4 °C | -30.0 °F | |
ConocoPhillips Hydroclear® MV150 AW Hydraulic Fluid Description: Conoco Hydroclear AW Hydraulic Fluid is specifically designed for use in high-pressure systems which require greater wear protection and deposit control than that provided by standard a.. |
|||
Pour Point | -34.4 °C | -30.0 °F | |
ConocoPhillips Hydroclear Diamond Class® 68 Turbine Oil Diamond Class Turbine Oil is a premium quality, rust and oxidation (R&O)-inhibited turbine oil developed for use in gas turbines and steam turbines in severe service. It is specially formulated to p.. |
|||
Pour Point | -34.4 °C | -30.0 °F | |
ConocoPhillips Hydroclear® 100 3 EP gear Oil Description: Conoco Hydroclear EP Gear Oil is a premium extreme-pressure industrial gear lubricant with superior deposit control. Hydroclear EP Gear Oil is specially formulated with proprietary addi.. |
|||
Pour Point | -34.4 °C | -30.0 °F | |
ConocoPhillips Hydroclear® 3 Ultra-clean multi-purpose R&O Oil, AGMA Lubricant No. 3 Description: Conoco Hydroclear Ultra-Clean Multipurpose R&O Oil is a rust- and oxidation-inhibited industrial oil with ashless wear protection formulated from premium Conoco hydrocracked base stocks.. |
|||
Pour Point | -34.4 °C | -30.0 °F | |
ConocoPhillips Hydroclear® 32 Rock Oil Description: Conoco Hydroclear Rock Drill Oil is a high-quality, heavy-duty, extreme-pressure pneumatic tool lubricant formulated from premium Conoco hydrocracked base stocks. Hydroclear Rock Drill .. |
|||
Pour Point | -34.4 °C | -30.0 °F | |
ConocoPhillips Hydroclear® 46 AW Hydraulic Fluid Description: Conoco Hydroclear AW Hydraulic Fluid is specifically designed for use in high-pressure systems which require greater wear protection and deposit control than that provided by standard a.. |
|||
Pour Point | -34.4 °C | -30.0 °F | |
ConocoPhillips Hydroclear® 46 Rock Oil Description: Conoco Hydroclear Rock Drill Oil is a high-quality, heavy-duty, extreme-pressure pneumatic tool lubricant formulated from premium Conoco hydrocracked base stocks. Hydroclear Rock Drill .. |
|||
Pour Point | -34.4 °C | -30.0 °F | |
ConocoPhillips Hydroclear® 68 Rock Oil Description: Conoco Hydroclear Rock Drill Oil is a high-quality, heavy-duty, extreme-pressure pneumatic tool lubricant formulated from premium Conoco hydrocracked base stocks. Hydroclear Rock Drill .. |